Preparation and characterization of lithium-ion-conductive Li1.3Al0.3Ti1.7(PO4)3 thin films by the solution deposition

2003; Elsevier BV; Volume: 425; Issue: 1-2 Linguagem: Inglês

10.1016/s0040-6090(02)01094-5

ISSN

1879-2731

Autores

Xian Wu, Xin Hai Li, Shao Wei Wang, Zhuo Wang, Yun He Zhang, Ming Xu, Ze He,

Tópico(s)

Ferroelectric and Piezoelectric Materials

Resumo

Li1.3Al0.3Ti1.7(PO4)3 thin films were successfully prepared by the solution deposition using lithium acetate, aluminum nitrate, ammonium dihydrogen phosphate and titanium butoxide as starting materials. The structure, surface morphology, electrochemical window, and ionic conductivity of the films were studied by X-ray diffraction, scanning electron microscopy, cyclic voltammetry and AC impedance. The results showed that Li1.3Al0.3Ti1.7(PO4)3 thin films annealed between 750 °C and 900 °C prepared by this method were well crystallized, homogenous and crack-free. The electrochemical window was beyond 2.4 V and the ionic conductivity was approximately 1.57×10−5 S/cm at room temperature for the film annealed at 800 °C for 30 min.

Referência(s)
Altmetric
PlumX