Strong hysteresis near solidification points of alkali halides with high ionic-radii ratios
1993; American Physical Society; Volume: 48; Issue: 2 Linguagem: Inglês
10.1103/physrevb.48.1280
ISSN1095-3795
AutoresA. Voronel, E. Shasha, D. Linsky, S. Feldberg,
Tópico(s)Solid-state spectroscopy and crystallography
ResumoA series of conductance measurements of alkali halides NaCl, NaBr, and NaI was performed in a range of 600--1100 K including liquid and solid states for both cooling and heating regimes. The hysteresis phenomenon is observed to be more pronounced for salts with higher ionic-radii ratio (200 K for NaI) with relaxation time exceeding hundreds of hours. At the cooling regime the conductivity drops slowly from a high value typical for liquids at the freezing point to a solid-salt value defined by a ${\mathrm{Na}}^{+}$ migration energy at the end of the hysteresis interval instead of an abrupt jump expected at the usual first-order transition. A sort of glassification is assumed to be present at the solidification interval of the salts with high ionic-radii ratios.
Referência(s)