SiC/Si3N4 nano/micro-composite — processing, RT and HT mechanical properties

2000; Elsevier BV; Volume: 20; Issue: 4 Linguagem: Inglês

10.1016/s0955-2219(99)00176-4

ISSN

1873-619X

Autores

Pavol Šajgalı́k, Miroslav Hnatko, František Lofaj, Pavol Hvizdoš, Ján Dusza, Peter Warbichler, Ferdinand Hofer, Ralf Riedel, Emmanuel Lecomte, Michael J. Hoffmann,

Tópico(s)

Aluminum Alloys Composites Properties

Resumo

Two SiC/Si3N4 nano/micro composites were prepared from a starting mixture of crystalline α-Si3N4, amorphous SiNC, Y2O3 and/or Al2O3. The composite material for room temperature (RT) application has high strength of 1200 MPa, Weibull modulus of 19 and moderate fracture toughness of 7 MPa m1/2. The composite for high temperature (HT) application, without Al2O3 has RT strength of 710 MPa and is able to keep 60% of its RT strength up to 1300°C. The creep resistance of composite material is approx. 1 order higher compared to relative monolith up to 1400°C.