Artigo Acesso aberto Revisado por pares

Microstructure and mechanical behavior of cast Ti-6Al-4V with addition of boron

2012; De Gruyter; Volume: 2; Issue: 3 Linguagem: Inglês

10.2478/s13531-012-0004-6

ISSN

2391-5439

Autores

Robert Pederson, Raghuveer Gaddam, Marta‐Lena Antti,

Tópico(s)

Advanced materials and composites

Resumo

Abstract The effect of boron (between 0.06 and 0.11 wt%) on the microstructure, hardness and compression properties of cast Ti-6Al-4V was investigated. Compression properties were examined in the temperature range from room temperature to 1000°C. It was found that the addition of boron refines the as-cast microstructure in terms of prior beta grain size and alpha colony size. This microstructural refinement led to an increase in compressive yield strength from room temperature up to 700°C. Three different strain rates (0.001, 0.1 and 1 s−1) were evaluated during compression testing from which it was found that the compressive yield strength decreased with decreasing strain rate from 600°C up to the beta transus temperature.

Referência(s)