Chemical Leaching on Sulfur and Mineral Matter Removal from Asphaltite (Harbul, SE Anatolia, Turkey)
2010; Taylor & Francis; Volume: 33; Issue: 5 Linguagem: Inglês
10.1080/15567030903030682
ISSN1556-7230
AutoresAbdurrahman Saydut, M. Zahir Düz, Serkan Erdoğan, Yalçın Tonbul, Candan Hamamcı,
Tópico(s)Drilling and Well Engineering
ResumoAbstract Desulfurization and demineralization by an aqueous caustic leaching method was investigated of an asphaltite sample from Harbul (Silopi, SE Anatolia, Turkey). The effects of different parameters, such as alkali concentration, time, and temperature, on the leaching efficiency were detailed and the experimental results are presented here. The caustic concentration varied from 0.1–1.0 M, temperature was 100–180°C, and leaching time varied from 4–16 h. The removal of total sulfur and ash increases with increasing alkali concentration, leaching temperature, and time. As a result of aqueous caustic leaching, the ash content of asphaltite was reduced from 32.49 to 18.00%, and 76% of combustible was recovered. Total sulfur and volatile matter content was reduced from 7.02 to 2.68% and from 46.74 to 25.10%, respectively. Keywords: alkali treatmentasphaltitecoaldemineralizationdesulphurization
Referência(s)