Frequency and temperature dependence of actuating performance of Bi1/2Na1/2TiO3-BaTiO3 based relaxor/ferroelectric composites

2014; American Institute of Physics; Volume: 115; Issue: 23 Linguagem: Inglês

10.1063/1.4876680

ISSN

1520-8850

Autores

Claudia Groh, Wook Jo, Jürgen Rödel,

Tópico(s)

Multiferroics and related materials

Resumo

Recently, composites of relaxors (matrix) and either ferroelectric or nonergodic relaxor (seed) were proposed as a solution to resolving one of the main drawbacks of incipient piezoceramics, namely the requirement for high driving electric fields. In this study, we investigate the temperature and frequency dependence of the actuating performance of Bi1/2Na1/2TiO3-BaTiO3-based composites. Apart from the reduction of driving field, the composite architecture offers an extra degree of freedom for tailoring the temperature stability for different operational conditions for actuators. High strain values appear to be sensitive especially to driving frequency. This is originated by the time-dependent process of the coalescence of polar nanoregions. In effect, proximity of driving field and poling field leads to high strain sensitivity. Hence, the driving electric field needs to be adjusted in order to meet the desired frequency specifications for given applications.

Referência(s)