Preparation and in vitro degradation of porous three-dimensional silk fibroin/chitosan scaffold

2008; Elsevier BV; Volume: 93; Issue: 7 Linguagem: Inglês

10.1016/j.polymdegradstab.2008.04.001

ISSN

1873-2321

Autores

Zhending She, Bofeng Zhang, Chenrui Jin, Qingling Feng, Yingxin Xu,

Tópico(s)

Bone Tissue Engineering Materials

Resumo

Degradation behaviors of porous scaffolds play an important role in the engineering process of a new tissue. In this study, three-dimensional porous silk fibroin/chitosan (SFCS) scaffolds were successfully prepared by freeze-drying method. In vitro degradation behaviors of SFCS scaffolds have been systematically investigated up to 8 weeks in phosphate buffer saline (PBS) solution at 37 °C. The following properties of the scaffolds were measured as a function of degradation time: pore morphology, structure, weight loss, and wet/dry weight value. The pH value of the PBS solution during degradation was also detected. SFCS scaffolds maintained its porous structure till 6 weeks of degradation. During the first 2 weeks, the pH value fluctuated in a narrow range from 6.53 to 6.93. SFCS scaffolds degraded much more quickly during the first 2 weeks, and the weight loss reached 19.28 wt% after 8 weeks of degradation. The degradation process affects little SFCS scaffolds' swelling properties.

Referência(s)