Laboratory investigations on the kinetics of gold electrowinning from acidic thiourea solutions containing alcohol admixture which can be obtained by gold elution from activated carbon in the processing of gold-bearing raw materials have been carried out as depending on temperature, current intensity and type of the cathode material. It has been found that a high gold recovery (96%–100%) can be obtained under suitable conditions (especially at elevated temperature of 60°C). The current efficiencies in the experimental conditions were in the range of 0.5%–1% and the energy consumption can be less than 15 kW h kg−1 of gold using a platinum mesh cathode.