Formation of AlVO 4 Solid Solution from Alkoxides

1987; Wiley; Volume: 70; Issue: 8 Linguagem: Inglês

10.1111/j.1151-2916.1987.tb05725.x

ISSN

1551-2916

Autores

Osamu Yamaguchi, Tatsuji Uegaki, Yutaka Miyata, Kiyoshí Shimizu,

Tópico(s)

Industrial Gas Emission Control

Resumo

Solid solutions of AlVO 4 crystallize at lower temperatures than amorphous materials between 50 and 70 mol% Al 2 O 3 prepared by the simultaneous hydrolysis of aluminum and vanadyl alkoxides. They decompose into α‐Al 2 O 3 , and V 2 O 5 , at 775° to 800°C. The compound AlVO 4 prepared from 50 mol% Al 2 O 3 has a triclinic unit cell with a = 0.6471 nm, b = 0.7742 nm, c = 0.9084 nm, α= 96.848°, β= 105.825°, and γ= 101.399°. The volume of the unit cell increases continuously with increases in Al 2 O 3 content. The structure contains tetrahedral AlO 4 , octahedral AlO 6 , and tetrahedral VO 4 groups.