Cyclic Fatigue Resistance of OneShape, HyFlex EDM, WaveOne Gold, and Reciproc Blue Nickel-titanium Instruments

2017; Elsevier BV; Volume: 43; Issue: 7 Linguagem: Inglês

10.1016/j.joen.2017.03.009

ISSN

1878-3554

Autores

Mustafa Gündoğar, Taha Özyürek,

Tópico(s)

Drilling and Well Engineering

Resumo

•We compared the fatigue resistance of the novel Reciproc Blue nickel-titanium instrument with HyFlex EDM, WaveOne Gold, and OneShape single-file NiTi instruments. •HyFlex EDM files were found to have statistically significantly higher cyclic fatigue resistance than Reciproc Blue, WaveOne Gold, and OneShape files (P < .05). •Reciproc Blue showed statistically higher resistance to static cyclic fatigue compared with WaveOne Gold files (P < .05). •In vivo studies are needed in order to determine the clinical performance of Reciproc Blue files. Introduction The purpose of this study was to compare the cyclic fatigue resistances of Reciproc Blue (VDW, Munich, Germany), HyFlex EDM (Coltene/Whaledent, Altstätten, Switzerland), WaveOne Gold (Dentsply Maillefer, Ballaigues, Switzerland), and OneShape (Micro Mega, Besancon, France) single-file NiTi systems. Methods Thirty Reciproc Blue R25 (25/.08), 30 HyFlex EDM (25/.∼), 30 WaveOne Gold Primary (25/.07), and 30 OneShape (25/.06) instruments were included in this study. All the instruments were rotated in artificial canals, which were made of stainless steel with an inner diameter of 1.5 mm, a 60° angle of curvature, and radii of curvatures of 5 mm until fracture occurred, and the time to fracture was recorded in seconds using a digital chronometer. The data were analyzed statistically using Kruskal-Wallis and post hoc Dunn tests via SPSS 21.0 software (SPSS Inc, Chicago, IL). The statistical significance level was set at 5%. Results The HyFlex EDM file (3456.33 ± 633.37) file had the statistically highest fatigue resistance, and the OneShape file (1221.63 ± 812.4) had the least fatigue resistance (P < .05). The mean number of cycles to fracture of the Reciproc Blue file (2875.89 ± 105.35) file was statistically higher than the WaveOne Gold file (1737.00 ± 376.32) (P < .05). There was no statistically significant difference (P > .05) in the mean length of the fractured fragments of the files (P > .05). Conclusion Within the limitations of the present in vitro study, it was found that cyclic fatigue resistance of HyFlex EDM files was higher than the cyclic fatigue resistances of OneShape, Reciproc Blue, and WaveOne Gold files.

Referência(s)
Altmetric
PlumX